MIL-DTL-23053/17B
TABLE II.
Physical properties.
1/ - Continued
Characteristic
Requirement
Test procedure and conditions
1014
Volume resistivity,
4.6.2 ASTM D876
ohm-cm, minimum
Dielectric constant,
3.7
4.6.2 ASTM D150
maximum
Specific gravity,
1.35
4.6.2 ASTM D792
maximum
Water absorption,
0.5
4.6.2 ASTM D570, 24 hrs.
percent, maximum
at 23°C
Corrosion
No corrosion
4.6.10.1 and 4.6.10.2
120° ± 2°C (248° ± 4°F),
16 hours
Low temperature
No cracking
4.6.7.1 -55° ± 1°C
flexibility
(-67° ± 2°F)
Flammability
Self-extinguish-
4.6.14 Procedure A
ing within 15
ASTM D2671
seconds; 3 inches
Heat resistance,
4.6.9 150° ± 2±C
property after:
(302° ± 4°F), 168 hours
Ultimate elongation,
100
percent, minimum
Fluid resistance,
4.6.11
property after:
Tensile strength,
1000(6.9)
psi (MPa), minimum
Elongation, percent,
100
minimum
Dielectric strength,
500(12.7)
volt/roil (Kv/mm),
minimum
Fungus resistance
4.6.2 ASTM G21
Non-nutrient
4