MIL-DTL-23053/6D
TABLE II. Physical Properties. 1/ - Continued
Characteristic
Test procedure and condition
Requirement
Ultimate elongation,
200
4.6.13 ASTM D638, 2
percent, minimum
inches/minute
Dielectric strength
500 (19.7)
4.6.2 ASTM D2671
volts/mil (Kv/mm),
minimum
1014
4.6.2. ASTM D876
Volume resistivity,
Ohm-cm, minimum
Dielectric constant,
4.6.2 ASTM D150
Class 1 - 3.2;
maximum 3/
Class 2 - 2.7
Class 1 - 1.35;
Specific gravity,
4.6.2 ASTM D792
Class 2 - 1.00
maximum
Class 1 - 0.5;
Water absorption,
4.6.2 ASTM D570, 24 hrs at
percent, maximum
Class 2 - 0.2
23°C
Corrosion
No corrosion
4.6.10.1 and 4.5.10.2,
150° ± 2°C (302° ± 4°F),
16 hours
No cracking
Low temperature
4.6.7.1 -55° ± 1°C
flexibility
(-67° ± 2°F)
Heat resistance,
properties after:
4.6.9 175° ± 2°C
(347° ± 4°F) for 168 hours
Ultimate elongation,
100
percent, minimum
4.6.11
Fluid resistance,
properties after:
Tensile strength,
1,600(11.1)
psi (MPa), minimum
Dielectric strength,
400 (15.8)
volts/roil (Kv/mm),
minimum
4